Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced N3WG6 LS BK - PA9T-GF30 - BASF

Material Data Center offers the following functions for Ultramid® Advanced N3WG6 LS BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Partially aromatic, glassfiber reinforced polyphthalamide for injection molding with strong mechanical properties especially at elevated temperatures, good long-term thermal stability and outstanding chemical resistance for highly stressed parts. The product can be characterized as compound with high toughness, stiffness, extremely low water absorption and outstanding dimensional stability. It features high flowability and allows filling of complex parts with thin wall thickness. The product is easily processable with excellent melt stability.

Markets & applications
Automotive: Fuel system, cooling system, powertrain, Auto E&E, sensors, fuel cell
E&E: Connectors
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
성형 수축률, 평행 0.5 / * % ISO 294-4, 2577
성형 수축률, 수직 1.0 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 10000 / 10000 MPa ISO 527
파단시 강도 190 / 175 MPa ISO 527
파단시 신율 2.4 / 2.2 % ISO 527
챠피 충격 강도 , +23°C 60 / 50 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 60 / 50 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 8 / 7 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 8 / 7 kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 300 / * °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 120 / * °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 270 / * °C ISO 75-1/-2
비카트 연화 온도, B 280 / * °C ISO 306
두께 H인 제품의 난연성 HB / * class IEC 60695-11-10
테스트 두께 0.8 / * mm -
전기적 특성건조/응축단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 4 / 3.6 - IEC 62631-2-1
소산 인자, 1MHz 105 / 205 E-4 IEC 62631-2-1
표면 저항 * / >1E15 Ohm IEC 62631-3-2
CTI - / 600 - IEC 60112
기타 특성건조/응축단위시험규격
물에서의 흡수성 2 / * % ISO 62와 유사
조건에서의 흡습성 0.9 / * % ISO 62와 유사
밀도 1370 / - kg/m³ ISO 1183
물질의 비성질건조/응축단위시험규격
ISO 데이터
점도수 100 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 120 °C -
Pre-drying - Time 8 h -
Processing humidity ≤0.05 % -
용융수지온도 320 - 340 °C -
성형온도 100 - 160 °C -
도표
동전단탄성율-온도 , Ultramid® Advanced N3WG6 LS BK (건조), PA9T-GF30, BASF
동전단탄성율-온도 , Ultramid® Advanced N3WG6 LS BK (응축), PA9T-GF30, BASF
응력-신율 , Ultramid® Advanced N3WG6 LS BK (건조), PA9T-GF30, BASF
응력-신율 , Ultramid® Advanced N3WG6 LS BK (응축), PA9T-GF30, BASF
시컨트탄성율-신율 , Ultramid® Advanced N3WG6 LS BK (건조), PA9T-GF30, BASF
시컨트탄성율-신율 , Ultramid® Advanced N3WG6 LS BK (응축), PA9T-GF30, BASF
인장탄성율-온도 , Ultramid® Advanced N3WG6 LS BK (건조), PA9T-GF30, BASF
인장탄성율-온도 , Ultramid® Advanced N3WG6 LS BK (응축), PA9T-GF30, BASF
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 검정
특별 특성
열안정성
특성
Melt Strength, Thermal Stability
내화학성에
General Chemical Resistance
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 320 - 340 °C
injection molding, Melt temperature, recommended: 330 °C
injection molding, Mold temperature, range: 125 - 170 °C
injection molding, Mold temperature, recommended: 140 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.